Standard Lanka Rubber (SLR L)

Product ID: P02-2

Send Inquiry
Manufactured using filed rubber latex and according to the international specifications. Identical in all respects to SMR L.
No. # SLR F/P SLR SP10 SLR H/M SLR L SLR L/N SLR Skim Grade SLR Y
% Dirt(Max) 0.02 - 0.03 0.03 0.5 0.10 0.10
% VM(Max) 0.6 0.6 0.6 0.6 0.6 0.6 0.6
% Ash(Max) 0.5 0.75 0.3 0.5 0.1 0.1 0.75
% Nitrogen 0.5 Max - 0.5 Max 0.5 Max 0.1 Max 0.6 Min 0.6 Max
P0 (Min) 30.0 40.0 30.0 30.0 30.0 40.0 30.0
PRI (Min) 60.0 60.0 60.0 60.0 60.0 60.0 50.0
Color low bond Grayish Brown No. # No. # No. # Gray Brown Yellowish Brown
Units No. # 3.0 3.0 3.9 No. 3 No. # No. #
Relax Modulus (NR 100) - - 6.5 6.0 6.0 8.5 8.0
Acetone Extract(Max) % 3.0 - 3.0 3.5 3.5 - 8.0
% Rebound Resilience(min) - - - - 80.0 - -
Level of Residual Toxins No1 - No 1 - - - -
Soluble Protein Content (Max) 0.05 - - - - - -
Specifications
  • Dirt (retained on 44 micron mesh) %wt: 0.021
  • Ash % wt: 0.18
  • Volatile matter % wt: 0.28
  • Nitrogen % wt: 0.33
  • Initial Wallace Plasticity (Po): 45.0
  • PRI (Pao/Po) x 100: 78.0
  • Lovibond Color Index: 1.5
Features
  • F/P: Food and pharmaceutical grade
  • SP: Superior Processed
  • H/M: High Money Viscosity
  • L/N: Low Nitrogen
  • Y: Yellow Fraction

Main Products

centrifuged latex, pale crepe rubber and foam mattresses